Yellow Rubber Group recently through technology, equipment, technical adjustments, shortening the vulcanization semi-fetal and steel products fetal test time and improve the specifications of the steel-fetal sulfide productivity.
Recently, the group of experts abroad with the help of semi-steel-fetal reduction to work to improve the fetal semi-steel production. After more than 20 groups and high-speed tire durability test, showed that in addition to some small tire, the big steel specifications semi-fetal sulfide productivity can be increased by 25 percent or more. Currently, when curing shrinkage has entered trial production stage, the first batch of pilot production specifications of the Steel Group semi-fetal current yield of more than 50 percent.
According to the group technical staff, in the course of trial production, they will continue to randomly selected fetal testing, if not quality problems, the next step will be carried out on other tire test at the reduction. All specifications to be adopted by all the tire test, in accordance with the new process will be formally put into production conditions. By then, half of the total annual production capacity fetal can increase more than 25 percent, the average Nissan up 7,500 more. |
|
|
 |